{"version":"1.0","provider_name":"Rainbow Dash Network","provider_url":"http:\/\/rainbowdash.net\/","type":"link","title":"adiwan (adiwan)'s status on Thursday, 20-Mar-25 17:06:43 UTC","author_name":"adiwan (adiwan)","author_url":"http:\/\/rainbowdash.net\/adiwan","url":"http:\/\/rainbowdash.net\/notice\/5483735","html":"I found the real culprit. It was a blob of PETG in the middle of the heat break. It was too far to be melted properly but close enough to let through a teeny tiny bit. It blocked the filament going through the nozzle at the expected rate. I tried to drill out the blob but I damaged the heat break and some of the threads in the heat block. Could have find it out sooner but the few days ago I couldn't be bothered to fully disassemble the hotend. As soon as the replacement arrives the assembly should be fairly quick. I can reuse the thermistor and heat cartridge. And the over all geometry and screw points should be the same too."}